Amalgam Creep Tester ADA Spec. No. 1


Information: Amalgam creep tester has been designed to test creep of dental amalgam materials as per ADA specification no. 1 for allow for dental amalgam. Instrument has been built in a solid aluminum block containing two amalgam specimens test stations where the temperature of 37 degrees Celsius is precisely controlled with a digital microprocessor controller and a designated creep test weight is applied onto the specimens through a designed cantilever mechanism. The creep of the specimen is detected by the 2-LVDT transducers which are connected to the two pen strip chart recorder for the creep test evaluation and analysis.

Instrument Spotlight